Still deciding? Get samples of $ !
Request Sample
|
| Customization: | Available |
|---|---|
| Type: | E (Carbon Steel Electrodes/ Low Alloy Steel Electrodes) |
| Material: | Carbon Steel |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
| Introduction: Low hydrogen electrode depositing 2.25Cr - 1Mo weld metal, display remarkable o strength and creep resistance at elevated temperatures up to 575 C. It is used for welding 21⁄4 Cr-1 Mo creep resistant steel and Cr-Mo-V steels resistant to hydrogen under pressure as well as for cast steels of a similar composition to the weld metal. |
|||||||||||||||||
Applications: Typical applications include steam boiler construction, welding of steam and super- heater piping, power plants, oil refinery and chemical plants. |
|||||||||||||||||
Chemical Composition of Deposited Metal (%)
|
|||||||||||||||||
Mechanical Properties of Deposited Metal
|
|||||||||||||||||
Diffusible Hydrogen Content in Deposited Metal: ≤4.0ml/100g(Glycerine Hydrogen Test) |
|||||||||||||||||
X-ray Radiographic Inspection: Grade I |
|||||||||||||||||
Reference Current (DC+)
|
|||||||||||||||||
Instructions: 1.The electrodes must be baked under about 350ºC for an hour before welding, and used as soon as baking is completed. 2.The stains on the weld, such as rust, oil stains, moisture, etc., must be cleared away before welding. |
|||||||||||||||||




| Packing & Delivery |
| FAQ |
Q: what is delivery time / lead time ?
A: 2-3weeks.
Q: what is your minimum order ?
A: 5000kgs/each size.
Q: what is your payment term ?
A: 50% T/T in advance, 50% balance paid before shipment.
Q: can we visit your factory ?
A: Yes, welcome to our factory at any time.\